HOME > SUPPORT > Q&A
Support
Q&A
 
 
Date : 26-07-10 16:25
Do you execute flattening, flaring, and reverse-flattening tests on every single manufacturing lot?
 
 Author : ひまり
Count : 301  
Yes, mechanical ductility verifications are performed on samples from every heat-treatment batch according to ASTM A1016.